Plastic waste, especially HDPE, has a very long decomposition time and has the potential to pollute the environment. Therefore, this study aims to determine the effect and most optimal variation of the addition of plastic bottle waste on the compressive strength of K-175 quality concrete. The experimental method was used by testing materials and compressive strength of concrete at the Ketapang State Polytechnic Laboratory from May to August 2024. The test results showed that the average compressive strength of normal concrete based on conversion to 28-day age reached 176.37 kg/cm², while the compressive strength of concrete with HDPE variations decreased with values ranging from 124.95 kg/cm² to 152.60 kg/cm². Of the various variations tested, the mixture with 0.75% HDPE showed the best compressive strength results compared to other variations, with an average compressive strength based on conversion to 28 days of age of 152.60 kg/cm².
Keyword: concrete compressive strength, HDPE plastic bottle waste, waste utilization
Downloads
Published
Issue
Section
Citation Check
License
- Authors retain copyright and grant the journal right of first publication with the work simultaneously licensed under a Creative Commons Attribution-ShareAlike 4.0 International License that allows others to share and adapt the work with an acknowledgement of the works authorship and initial publication in this journal.
- Authors are able to enter into separate, additional contractual arrangements for the non-exclusive distribution of the journals published version of the work (e.g., post it to an institutional repository or publish it in a book), with an acknowledgement of its initial publication in this journal.
- Upon receiving the proofs, the Author/Editor agrees to promptly check the proofs carefully, correct any errors, and authorize the publication of the corrected proofs.